Cold Work Tool Steel
-
AISI D6 Tool Steel | 1.2436 | X210CrW12 | SKD2 Cold Work Steel
D6 tool steel has the characteristics of high hardenability, hardenability, strength and toughness, wear resistance and small quenching volume deformation.
Email Details
D6 tool steel is suitable for cold stamping die, wire drawing die, drawing die, embossing die, wire rolling die, wire rolling plate, cold upsetting die and cold extrusion die. -
Cr12MoV Tool Steel
Cr12MoV steel is suitable for blanking die steel, drawing die, thread rolling die, thread rolling plate, and die with complex shape and impact load.
Email Details -
Hot
X12MΦ Tool Steel
X12MΦ The steel is suitable for punching die, cold extrusion die, thread rolling wheel, thread rolling wheel, cold shear knife and precision measuring tools with complex shapes.
Email Details -
1.2436 Tool Steel
1.2436 steel is suitable for medium load stamping die, stamping stainless steel, copper, silicon, aluminum, etc.
Email Details -
1.2510 Tool Steel
1.2510 steel is suitable for making wear-resistant and non deformed cold working dies, jewelry embossing dies, various metal stamping dies and forming tools, mold bushings and cutting tools.
Email Details -
D6 Tool Steel
D6 steel is mainly used for cold stamping dies and punches, cold cutting scissors, drill sleeves, gauges, wire drawing dies, stamping dies, thread take-up plates, drawing dies and thread rolling dies, which bear small impact loads and require high wear resistance.
Email Details -
O1 Tool Steel | 1.2510 | 100MnCrW4 | SKS3
O1 mold steel is widely used. O1 steel has good processability, good wear resistance, stable O1 heat treatment performance, small dimensional deformation, but weak toughness and corrosion resistance. It is commonly used in blanking die, punching die, punching die, punching die, etc.
Email Details -
1.2842 Tool Steel
1.2842 tool steel is suitable for manufacturing all kinds of precision measuring tools and templates. It is also used for stamping dies, cold pressing dies, engraving dies, blanking dies, etc. with relatively small size. It can also be used as structural parts such as screw rods of machine tools. It is used to manufacture all kinds of cold punching dies and tools with large section, complex shape and heavy working conditions, such as punching die, trimming die, edging die, deep drawing die of steel plate, circular saw, standard tools and gauges, thread rolling die, etc.
Email Details -
O2 Tool Steel
O2 tool steel is suitable for manufacturing all kinds of precision measuring tools and templates. It is also used for stamping dies, cold pressing dies, engraving dies, blanking dies, etc. with relatively small size. It can also be used as structural parts such as screw rods of machine tools. It is used to manufacture all kinds of cold punching dies and tools with large section, complex shape and heavy working conditions, such as punching die, trimming die, edging die, deep drawing die of steel plate, circular saw, standard tools and gauges, thread rolling die, etc.
Email Details