d6
-
H12 Work Tool Steel
H12 hot working die steel has good heat resistance, good strength and hardness at high temperature, high wear resistance and toughness, and good thermal fatigue performance.
Email Details
H12 hot working die steel is generally recommended for hot working applications that require most crack resistance. These applications include hot punches, die casting molds, forming molds, hot scissors, hot fixture molds and extrusion tools. -
Hot
SKD61 Hot Work Tool Steel
SKD61 steel is suitable for hot work, aluminum, magnesium, zinc, copper alloy die-casting die, slotting cutter, scissors and hot forging action, plastic mold, hot work reamer, rolling cutter, general hot work forging die, hot bolt die, hot room tools, etc.
Email Details -
H13 Tool Steel | 1.2344 | X40CrMoV5-1 | SKD61 Hot Work Steel
H13 hot working die steel. It has excellent machinability and polishing performance, high toughness and plasticity, good high and low temperature wear resistance, high temperature fatigue and heat resistance.
Email Details
H13 tool steel can be used for die forging hammer forging die, aluminum alloy die casting die, hot extrusion die, high-speed precision forging die and forging press die, etc. -
AISI D6 Tool Steel | 1.2436 | X210CrW12 | SKD2 Cold Work Steel
D6 tool steel has the characteristics of high hardenability, hardenability, strength and toughness, wear resistance and small quenching volume deformation.
Email Details
D6 tool steel is suitable for cold stamping die, wire drawing die, drawing die, embossing die, wire rolling die, wire rolling plate, cold upsetting die and cold extrusion die. -
D6 Tool Steel
D6 steel is mainly used for cold stamping dies and punches, cold cutting scissors, drill sleeves, gauges, wire drawing dies, stamping dies, thread take-up plates, drawing dies and thread rolling dies, which bear small impact loads and require high wear resistance.
Email Details -
AISI H11 Tool Steel | 1.2343 | X37CrMoV5-1 | SKD6 | BH11
H11 air cooling hardening hot working die steel. H11 steel is one of the three most commonly used hot working die steels in the European die casting industry. The carbides in the steel are fine, evenly distributed, good cold and hot fatigue resistance and corrosion resistance, good cold and hot working performance, good hardenability, thick thermal strength, oxidation resistance, high toughness and wear resistance at medium temperature.
Email Details -
Cr12W Tool Steel
Cr12W steel is suitable for cold extrusion die, cold stamping die, wire rolling die, wire rolling plate, etc. with complex shape and high impact resistance.
Email Details