mould steel
-
K110 Tool Steel
K110 steel is suitable for heavy cutting tools, high-efficiency shearing cold stamping dies, cutting scissors, sheet cutting, circular hobs, deep drawing dies and cold extrusion dies.
Email Details -
H10 Hot Work Tool Steel
H10 tool steel can be used to make male and female dies with high stress under high temperature but not subject to impact load, such as concave and convex dies, inserts, copper alloy extrusion dies, die-casting dies, such as reverse extrusion dies, and hot metal cutters under high temperature.
Email Details -
A2 Tool Steel
A2 Tool Steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment.
Email Details -
9CrWMn Tool Steel
9crwmn steel is used to make cold stamping dies, jewelry embossing dies, cutting tools, etc. with small section and complex shape and high accuracy.
Email Details -
M42 High Speed Steel
M42 is a high-quality cobalt high-speed steel. Its chemical composition is designed for high hardness and excellent thermal hardness. These characteristics make the steel the best choice for machining high-strength and pre hardened steels, high hardness alloys and difficult to machine nonferrous metal superalloys used in aerospace, petroleum and power generation industries.
Email Details
Cutting tools made of M42 steel can cut iron-based superalloys, cast superalloys, titanium alloys and ultra-high strength steels. Because of its good grindability, it can be used to manufacture all kinds of high-precision and complex cutting tools. -
9Cr18Mo Plastic Mould Steel
9Cr18Mo steel is suitable for bearing, turbine blade, nozzle, valve, plate ruler, cutter and scissors with good corrosion resistance.
Email Details -
NC6 Tool Steel
NC6 is mainly used to produce cutting tools, tapping machines, chisels, drills, files, machine drills, cold stamping dies and die cutting plates. Medium hardness and high hardness steel, with good machinability and wear resistance. It is characterized by low tendency of bending and dimensional change during hardening, and low toughness and tempering resistance.
Email Details -
D3 Cold Work Steel | 1.2080 | X210Cr12 | SKD1
D3 steel has good wear resistance and is suitable for making dies and punches with low impact load and high wear resistance, cold shear knives, drill sleeves, gauges, wire drawing dies, etc.
Email Details