skh59 steel
-
M42 High Speed Steel
M42 is a high-quality cobalt high-speed steel. Its chemical composition is designed for high hardness and excellent thermal hardness. These characteristics make the steel the best choice for machining high-strength and pre hardened steels, high hardness alloys and difficult to machine nonferrous metal superalloys used in aerospace, petroleum and power generation industries.
Email Details
Cutting tools made of M42 steel can cut iron-based superalloys, cast superalloys, titanium alloys and ultra-high strength steels. Because of its good grindability, it can be used to manufacture all kinds of high-precision and complex cutting tools.